Nh - The Launch Thread, Godspeed little one |
Nh - The Launch Thread, Godspeed little one |
Jan 16 2006, 03:08 PM
Post
#1
|
|
Founder Group: Chairman Posts: 14448 Joined: 8-February 04 Member No.: 1 |
I thought it was time, with the Atlas V about to roll out - for a new thread for NH for the launch etc.
Someone asked over at the HZ just how NH can go so fast, this was my reply.... QUOTE How do you get a spacecraft to Jupiter in under a year? Easy. Make it very very light, and put it on a very very big rocket. The config of Atlas V rocket being used to launch NH (551 - 5m fairing, 5 solids, and one engine on the Centaur stage ) would typically put 8,670kg into GTO or 20,520 into LEO. New Horizons is 478kg, and it's Star 48B 3rd stage is 2,137kg - so instead of hauling 20 tons, this vehicle is hauling about 2.5 tons thus you get a HUGE velocity out of it. AND, once it's done that, you have the final kick of the 48B, 591 thousand kgs-s (thus accelerating is all a further 3.5 - 4km/s ball park speed, if my maths is right) At launch - the vehicle is 573,160kg. NH is 0.083% of it. Imagine the Apollo entry capsule on top of a Saturn V...tiny tiny tiny... that was 5,800 kg on a 3,038,500kg rocket - 0.191% - more than double that percentage of NH. The cutaway's are almost comical, with this tiny gold-clad box on an enormous vehicle. Basically - it's a LOT of rocket, and not a lot of payload. For comparison, look how much fuss was made of Stardust that entered so quickly. It took >16 hrs to get from the distance of the moon to Utah. NH makes that journey in 9 hours One thing the NH mission is not short of, is superlatives. I'm not one for good luck charms (although I'll eat peanuts during a Martian EDL with the best of them), but this mission has been so long in coming, that it deserves every ounce of luck it can have - the best, most accurate launch possible, the cleanest checkout, and incident free cruise to Jupiter. Goodluck and Godspeed little one, we're with you every step of the way. Doug PS - Alan, you're a credit to your field, spending so much time answering questions and writing the PI Perspectives, it's been a hell of a journey! |
|
|
Jan 16 2006, 10:16 PM
Post
#2
|
|
Member Group: Members Posts: 356 Joined: 12-March 05 Member No.: 190 |
dumb ? time. Why is the first stage copper clad?
|
|
|
Jan 16 2006, 11:18 PM
Post
#3
|
|
Member Group: Members Posts: 408 Joined: 3-August 05 Member No.: 453 |
|
|
|
Jan 16 2006, 11:41 PM
Post
#4
|
|
Forum Contributor Group: Members Posts: 1374 Joined: 8-February 04 From: North East Florida, USA. Member No.: 11 |
The first stage tank is Copper Anodised Aluminium.
" Anodising successfully combines science with nature to create one of nature's best metal finishes. It is an electrochemical process that thickens and toughens the naturally occurring protective oxide. The resulting finish, depending on the process, is the second hardest substance known to man, second only to diamond" |
|
|
Jan 17 2006, 12:07 AM
Post
#5
|
|
Member Group: Members Posts: 600 Joined: 26-August 05 Member No.: 476 |
QUOTE (MahFL @ Jan 16 2006, 03:41 PM) The first stage tank is Copper Anodised Aluminium. " Anodising successfully combines science with nature to create one of nature's best metal finishes. It is an electrochemical process that thickens and toughens the naturally occurring protective oxide. The resulting finish, depending on the process, is the second hardest substance known to man, second only to diamond" "Copper" anodized aluminum? I understand the anodizing process leaves a bonded coating of aluminum oxide. Is copper used as a descriptive adjective here, or is there actually copper involved? |
|
|
Jan 17 2006, 12:15 AM
Post
#6
|
|
Senior Member Group: Members Posts: 2547 Joined: 13-September 05 Member No.: 497 |
QUOTE (mchan @ Jan 16 2006, 04:07 PM) "Copper" anodized aluminum? I understand the anodizing process leaves a bonded coating of aluminum oxide. Is copper used as a descriptive adjective here, or is there actually copper involved? You can add dyes during the anodizing process and get most any color you like, but as I said before, I think it's more likely that the booster is chromate-conversion coated, because that would leave you with a natural golden-coppery color. But I couldn't find any confirmation in the Atlas documents I looked at. I can say for sure they didn't make the stage out of any AlBe or AlLi alloy, though. -------------------- Disclaimer: This post is based on public information only. Any opinions are my own.
|
|
|
Jan 17 2006, 12:28 AM
Post
#7
|
|
Member Group: Members Posts: 548 Joined: 19-March 05 From: Princeton, NJ, USA Member No.: 212 |
To Pluto and BEYOND !!!
at last !!!! and for those who missed it, The Science Channel Documentary on sunday night was quite enjoyable and there are a few more repeats. Here is a brief summary from my other thread. ---------------------------------------------------- The Discovery Science Channel is showing a documentary on the New Horizons mission which premieres on Sunday, Jan 15 at 9PM check this link: http://science.discovery.com/tvlistings/ep...d=0&channel=SCI Synopsis: Passport to Pluto NASA's New Horizons mission is exploring the "new frontier" of the outer reaches of our solar system, solving the mysteries of Pluto and beyond. Meet the scientists who have waited their whole lives for this mission and see what surprises they'll reveal |
|
|
Lo-Fi Version | Time is now: 31st October 2024 - 11:05 PM |
RULES AND GUIDELINES Please read the Forum Rules and Guidelines before posting. IMAGE COPYRIGHT |
OPINIONS AND MODERATION Opinions expressed on UnmannedSpaceflight.com are those of the individual posters and do not necessarily reflect the opinions of UnmannedSpaceflight.com or The Planetary Society. The all-volunteer UnmannedSpaceflight.com moderation team is wholly independent of The Planetary Society. The Planetary Society has no influence over decisions made by the UnmannedSpaceflight.com moderators. |
SUPPORT THE FORUM Unmannedspaceflight.com is funded by the Planetary Society. Please consider supporting our work and many other projects by donating to the Society or becoming a member. |